Tensile Strength, Yield 413 MPa

@Thickness 12.7 mm,
Temperature 316 °C
59900 psi

@Thickness 0.500 in,
Temperature 601 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..