Polymer Property : Tensile Strength, Yield = 44100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 304 MPa

@Strain 0.200 %,
Thickness 76.2 - 101.6 mm
>= 44100 psi

@Strain 0.200 %,
Thickness 3.00 - 4.000 in
Tempers T851/T852
Constellium Alumold® 350 Aluminum
Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti..