Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa

@Temperature 77.0 °C
6530 psi

@Temperature 171 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers