Mechanical Properties Metric English Comments
Tensile Strength, Yield 321 MPa

@Temperature 23.0 °C
46600 psi

@Temperature 73.4 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..