Tensile Strength, Yield 324 MPa

@Thickness 12.7 mm,
Temperature 371 °C
47000 psi

@Thickness 0.500 in,
Temperature 700 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield 324 MPa

@Temperature 23.0 °C
47000 psi

@Temperature 73.4 °F
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed
AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chl..