Mechanical Properties Metric English Comments
Tensile Strength, Yield 331 MPa

@Temperature 260 °C
48000 psi

@Temperature 500 °F
0° Direction, Dry; 325°F Autoclave Cured; ASTM D638
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Tensile Strength, Yield 331 MPa

@Thickness 1.57 mm
48000 psi

@Thickness 0.0620 in
CW; ASTM D638
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate
Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con..
Tensile Strength, Yield 331 MPa

@Thickness 3.17 mm
48000 psi

@Thickness 0.125 in
LW
Industrial Laminates/Norplex P95 Glass Fabric
Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested..
Tensile Strength, Yield 331 MPa

@Thickness 9.50 - 25.4 mm,
Temperature 204 °C
48000 psi

@Thickness 0.374 - 1.00 in,
Temperature 399 °F
0.2% offset
Haynes Hastelloy® S alloy, flat products
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 331 MPa

@Diameter 9.70 mm,
Temperature 25.0 °C
48000 psi

@Diameter 0.382 in,
Temperature 77.0 °F
0.2% offset
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..