Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.10 MPa

@Strain 100 %
740 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1080A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..