Polymer Property : Tensile Strength, Yield = 5.60 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.60 MPa

@Strain 100 %
812 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 2058A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 5.60 MPa

@Strain 300 %
812 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..