Mechanical Properties Metric English Comments
Tensile Strength, Yield 358 MPa

@Thickness 1.60 mm,
Temperature 20.0 °C
51900 psi

@Thickness 0.0630 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-2000® alloy, flat products
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield 358 MPa

@Strain 0.200 %
51900 psi

@Strain 0.200 %
Typical for Plate, Annealed, 2"
AK Steel NITRONIC® 30 Austenitic Stainless Steel
AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi..