Polymer Property : Tensile Strength, Yield = 52100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 303 - 359 MPa

@Strain 0.200 %
43900 - 52100 psi

@Strain 0.200 %
Typical
AK Steel 18 Cr-Cb™ Ferritic Stainless steel
AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili..