Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa

@Strain 300 %
5220 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® S60D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Yield 36.0 MPa

@Strain 100 %
5220 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® S74D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Yield 36.0 MPa

@Temperature 23.0 °C
5220 psi

@Temperature 73.4 °F
ASTM D638
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Tensile Strength, Yield 36.0 MPa

@Strain 100 %
5220 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® C-74D Polyester Type Polyurethane Elastomer