Polymer Property : Tensile Strength, Yield = 52600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 363 MPa

@Strain 0.200 %,
Temperature 540 °C
52600 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Tensile Strength, Yield 363 MPa

@Temperature 71.0 °C
52600 psi

@Temperature 160 °F
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel