Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 538 MPa @Temperature -196 °C |
78000 psi @Temperature -320 °F |
|
Crucible Steel 20 Cb Plus Stainless Steel Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack.. |