Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 371 MPa @Strain 0.200 %, Temperature 700 °C |
53800 psi @Strain 0.200 %, Temperature 1290 °F |
Bar |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 371 MPa @Thickness 1.70 mm, Temperature 316 °C |
53800 psi @Thickness 0.0669 in, Temperature 601 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |