Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.00 MPa

@Temperature 100 °C
870 psi

@Temperature 212 °F
50 mm/min; ISO 527-2
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r..
Tensile Strength, Yield 6.00 MPa

@Temperature 149 °C
870 psi

@Temperature 300 °F
Flatwise Tension
Hexcel® Redux® 322 Modified epoxy film adhesive (0.078 psf)
Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up ..