Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.86 MPa

@Strain 100 %
996 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 185A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 6.86 MPa

@Strain 300 %
996 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 870A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 6.86 MPa

@Strain 300 %
996 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 470A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..