Mechanical Properties Metric English Comments
Tensile Strength, Yield 415 MPa

@Thickness 1.57 mm
60200 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate
Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con..
Tensile Strength, Yield 415 MPa

@Thickness 12.7 mm,
Temperature 260 °C
60200 psi

@Thickness 0.500 in,
Temperature 500 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield >= 415 MPa

@Strain 0.200 %,
Thickness 80.0 - 100 mm
>= 60200 psi

@Strain 0.200 %,
Thickness 3.15 - 3.94 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength, Yield 415 MPa

@Strain 0.200 %
60200 psi

@Strain 0.200 %
Typical
Aleris Hokotol Aluminum Alloy, 325 mm Thickness
Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an..