Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 425 MPa @Thickness 1.57 mm |
61600 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP509 Glass Fabric Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc.. |
|||
Tensile Strength, Yield | >= 425 MPa @Strain 0.200 %, Temperature 350 °C |
>= 61600 psi @Strain 0.200 %, Temperature 662 °F |
|
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |