Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 463 MPa @Strain 0.200 % |
67100 psi @Strain 0.200 % |
11-15in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Tensile Strength, Yield | 463 MPa @Strain 0.200 % |
67100 psi @Strain 0.200 % |
15-17in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Tensile Strength, Yield | 463 MPa @Strain 0.200 % |
67100 psi @Strain 0.200 % |
7-11in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |