Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.55 MPa @Strain 300 % |
1100 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 400 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |