Mechanical Properties Metric English Comments
Tensile Strength, Yield 489.9 MPa

@Strain 0.200 %
71050 psi

@Strain 0.200 %
after porcelain firing
Wieland Euro 50 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental