Polymer Property : Tensile Strength, Yield = 73500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 507 MPa

@Strain 0.200 %
73500 psi

@Strain 0.200 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4501 Duplex Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 507 MPa

@Temperature 24.0 °C
73500 psi

@Temperature 75.2 °F
Warp TS
Hexcel® HexPly® F185 Epoxy Resin, K285 Kevlar Fabric
Hexcel designation: 285-38"-F185; Fiber: Kev. 49 1140Information provided by HexCel
Tensile Strength, Yield 507 MPa

@Strain 0.200 %,
Temperature 500 °C
73500 psi

@Strain 0.200 %,
Temperature 932 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..