Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 74000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 510 MPa

@Strain 0.200 %
74000 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Tensile Strength, Yield 510 MPa

@Diameter 12.7 mm,
Temperature 25.0 °C
74000 psi

@Diameter 0.500 in,
Temperature 77.0 °F
0.2% offset
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield >= 510 MPa

@Strain 0.200 %,
Temperature 150 °C
>= 74000 psi

@Strain 0.200 %,
Temperature 302 °F
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 510 MPa

@Strain 0.200 %,
Thickness 9.90 - 25.0 mm
74000 psi

@Strain 0.200 %,
Thickness 0.390 - 0.984 in
Typical Strength
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield 510 MPa

@Strain 0.200 %,
Thickness 152.4 - 203.2 mm
74000 psi

@Strain 0.200 %,
Thickness 6.000 - 8.000 in
Typical Strength
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength, Yield >= 510 MPa

@Strain 0.200 %
>= 74000 psi

@Strain 0.200 %
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom..
Copyright © lookpolymers.com All Rights Reserved