Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 530 MPa @Strain 0.200 %, Temperature 400 °C |
76900 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4313 Martensitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 530 MPa @Strain 0.200 % |
76900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4501 Duplex Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 530 MPa @Strain 0.200 % |
76900 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Yield | >= 530 MPa @Strain 0.200 %, Temperature 100 °C |
>= 76900 psi @Strain 0.200 %, Temperature 212 °F |
|
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | >= 530 MPa @Strain 0.200 %, Temperature 400 °C |
>= 76900 psi @Strain 0.200 %, Temperature 752 °F |
|
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | >= 530 MPa @Thickness >=65.0 mm |
>= 76900 psi @Thickness >=2.56 in |
|
ThyssenKrupp N-A-XTRA® M 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 530 MPa @Strain 0.200 %, Thickness 76.2 - 127 mm |
76900 psi @Strain 0.200 %, Thickness 3.00 - 5.00 in |
Typical Strength |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Tensile Strength, Yield | 530 MPa @Strain 0.100 %, Temperature 600 °C |
76900 psi @Strain 0.100 %, Temperature 1110 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |