Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.9 MPa @Thickness 3.20 mm |
8110 psi @Thickness 0.126 in |
Type I, 50 mm/min; ASTM D638 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 55.9 MPa @Thickness 3.20 mm |
8110 psi @Thickness 0.126 in |
Type I, 50 mm/min; ASTM D638 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |