Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 82.7 MPa @Thickness 1.57 mm |
12000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Tensile Strength, Yield | 82.7 MPa @Thickness 1.57 mm |
12000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP347 Cotton Fabric Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1.. |
|||
Tensile Strength, Yield | 82.7 MPa @Thickness 1.57 mm |
12000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Tensile Strength, Yield | 82.7 MPa @Thickness 3.17 mm |
12000 psi @Thickness 0.125 in |
CW |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Tensile Strength, Yield | 82.7 MPa @Thickness 1.57 mm |
12000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP691 Paper Base Laminate Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0... |