Polymer Property : Tensile Strength, Yield = 82700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 570 MPa

@Strain 1.00 %
>= 82700 psi

@Strain 1.00 %
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Tensile Strength, Yield >= 570 MPa

@Strain 1.00 %
>= 82700 psi

@Strain 1.00 %
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Tensile Strength, Yield >= 570 MPa

@Strain 0.200 %,
Temperature 150 °C
>= 82700 psi

@Strain 0.200 %,
Temperature 302 °F
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield >= 570 MPa

@Strain 0.200 %,
Temperature 300 °C
>= 82700 psi

@Strain 0.200 %,
Temperature 572 °F
ThyssenKrupp N-A-XTRA® 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 570 MPa

@Temperature 24.0 °C
82700 psi

@Temperature 75.2 °F
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel