Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 83.0 MPa @Temperature 23.0 °C |
12000 psi @Temperature 73.4 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 83.0 MPa @Temperature 23.0 °C |
12000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 83.0 MPa @Temperature 23.0 °C |
12000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |