Polymer Property : Tensile Strength, Yield = 831 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 831 MPa

@Strain 0.200 %,
Thickness 1.45 mm
121000 psi

@Strain 0.200 %,
Thickness 0.0571 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Tensile Strength, Yield 831 MPa

@Temperature 25.0 °C,
Time 45700 sec
121000 psi

@Temperature 77.0 °F,
Time 12.7 hour
As Welded and Aged at 1850°F(1010°C)/2hr/AC + 1450°F(788°C)/8h/AC; Weld/Weld Fracture; 0.2% Offset
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..