Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 578 MPa @Temperature 538 °C, Time 45700 sec |
83800 psi @Temperature 1000 °F, Time 12.7 hour |
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |