Polymer Property : Tensile Strength, Yield = 84.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 84.0 MPa

@Temperature 23.0 °C
12200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E41HSB NC010 Nylon 66  (Unverified Data**)
Zytel® E41HSB is an unreinforced, high viscosity, heat stabilized polyamide 66 for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 84.0 MPa

@Temperature 23.0 °C
12200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Zytel® E51HSB NC010 is a high molecular weight, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 84.0 MPa

@Temperature 23.0 °C
12200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66  (Unverified Data**)
Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 84.0 MPa

@Temperature 23.0 °C
12200 psi

@Temperature 73.4 °F
ASTM D638
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..
Tensile Strength, Yield 84.0 MPa

@Temperature 23.0 °C
12200 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66  (Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..