Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 841 MPa @Temperature 23.0 °C |
122000 psi @Temperature 73.4 °F |
AS4C; Fill Tension; (AMB) |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |