Mechanical Properties Metric English Comments
Tensile Strength, Yield 590 MPa

@Strain 0.200 %,
Temperature 100 °C
85600 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4313 Martensitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Tensile Strength, Yield 590 MPa

@Strain 0.200 %
85600 psi

@Strain 0.200 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Tensile Strength, Yield 590 MPa

@Strain 0.200 %,
Temperature 400 °C
85600 psi

@Strain 0.200 %,
Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield >= 590 MPa

@Strain 0.200 %,
Temperature 100 °C
>= 85600 psi

@Strain 0.200 %,
Temperature 212 °F
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 590 MPa

@Strain 0.200 %,
Temperature 800 °C
85600 psi

@Strain 0.200 %,
Temperature 1470 °F
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..