Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 627 MPa @Temperature -53.9 °C |
91000 psi @Temperature -65.0 °F |
0° Direction, Dry; Autoclave Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Strength, Yield | 627 MPa @Temperature 399 °C |
91000 psi @Temperature 750 °F |
Round bar 1" diameter, 310 HB |
EDRO #2 Prehardened 4130 Holder Block EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition. EDRO #2™ is characterized by excellent machinability, good resistance to i.. |
|||
Tensile Strength, Yield | 627 MPa @Temperature 399 °C |
91000 psi @Temperature 750 °F |
Round bar 1" diameter, 310 HB |
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |