Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 650 MPa @Strain 1.00 %, Temperature -196 °C |
94300 psi @Strain 1.00 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 650 MPa @Strain 0.200 % |
94300 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4313 Martensitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 650 MPa @Temperature 600 °C |
94300 psi @Temperature 1110 °F |
|
H.C. Starck Ampersint® MAP FeCoNi 40/20/40 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 650 MPa @Temperature 600 °C |
94300 psi @Temperature 1110 °F |
|
H.C. Starck Ampersint® MAP FeCoNi 70/10/20 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 650 MPa @Temperature 600 °C |
94300 psi @Temperature 1110 °F |
|
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 650 MPa @Temperature 600 °C |
94300 psi @Temperature 1110 °F |
|
H.C. Starck Ampersint® MAP FeNi 50/50 For Soft Magnets High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 650 MPa @Temperature 600 °C |
94300 psi @Temperature 1110 °F |
|
H.C. Starck Ampersint® MAP FeCo 50/50 For Soft Magnets High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Tensile Strength, Yield | 650 MPa @Temperature 25.0 °C, Time 45700 sec |
94300 psi @Temperature 77.0 °F, Time 12.7 hour |
As Welded, Solution Annealed, and Aged; Weld/Weld Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | >= 650 MPa @Thickness >=65.0 mm |
>= 94300 psi @Thickness >=2.56 in |
|
ThyssenKrupp N-A-XTRA® M 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |