Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 660.00 MPa

@Strain 0.200 %
95725 psi

@Strain 0.200 %
hardened
Wieland Auropal 2 Casting Alloy
Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental