Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.67 - 6.86 MPa

@Strain 50.0 %
967 - 996 psi

@Strain 50.0 %
ASTM D638
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec..