Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.00540 - 0.00556 MPa-m/sec
154 - 159 psi-ft/min
300 m/min
Polikim EFALON® C-25 PTFE, 25% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..