Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | (with 4:1 safety factor applied); QTM 55007 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 10 fpm |
Techmer ES Luriblend® TPX-HDPE-99018 Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc. |
|||
Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.105 - 0.430 MPa-m/sec | 3000 - 12300 psi-ft/min | Average value: 0.278 MPa-m/sec Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |