Polymer Property : Limiting Pressure Velocity = 0.233 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.233 MPa-m/sec
6650 psi-ft/min
v = 200m/min
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..