Polymer Property : Limiting Pressure Velocity = 0.400 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.400 MPa-m/sec
11400 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data)
This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica..
Limiting Pressure Velocity 0.400 MPa-m/sec
11400 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Limiting Pressure Velocity 0.400 MPa-m/sec
11400 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data)
FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application..
Limiting Pressure Velocity 0.400 MPa-m/sec
11400 psi-ft/min
v = 100m/min
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Limiting Pressure Velocity 0.400 MPa-m/sec
11400 psi-ft/min
v = 200m/min
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Limiting Pressure Velocity 0.400 MPa-m/sec
11400 psi-ft/min
v = 200m/min
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..