Limiting Pressure Velocity 0.43333 MPa-m/sec
12372 psi-ft/min
v = 100m/min
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..