Polymer Property : Limiting Pressure Velocity = 0.440 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.440 MPa-m/sec
12600 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data)
This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap..
Limiting Pressure Velocity 0.440 MPa-m/sec
12600 psi-ft/min
without lubrication; MPC Test
Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.