Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.480 MPa-m/sec | 13700 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |
|||
Limiting Pressure Velocity | 0.480 MPa-m/sec | 13700 psi-ft/min | v = 10m/min |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |