Polymer Property : Limiting Pressure Velocity = 0.525 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.525 MPa-m/sec
15000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Ketron® CM 1030HT PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products
Limiting Pressure Velocity 0.525 MPa-m/sec
15000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.525 MPa-m/sec
15000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.525 MPa-m/sec
15000 psi-ft/min
Unlubricated
TriStar Ultracomp UC-300 Composite Bearing
Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family..