Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.740 MPa-m/sec
21100 psi-ft/min
Kuraray Genestarâ„¢ N1006D-H31 Nylon
Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications