Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.771 - 3.30 MPa-m/sec | 22000 - 94200 psi-ft/min | Average value: 1.45 MPa-m/sec Grade Count:5 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Limiting Pressure Velocity | 0.771 MPa-m/sec | 22000 psi-ft/min | 1000 fpm |
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: .. |
|||
Limiting Pressure Velocity | 0.771 MPa-m/sec | 22000 psi-ft/min | 1000 fpm |
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro.. |
|||
Limiting Pressure Velocity | 0.771 MPa-m/sec | 22000 psi-ft/min | 1000 fpm |
Techmer ES Luriblend® PA6/6 CF30 TL12 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: Lubricated and Good Wear ResistanceTPCI# 6466101Inf.. |
|||
Limiting Pressure Velocity | 0.771 MPa-m/sec | 22000 psi-ft/min | 1000 fpm |
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance.. |
|||
Limiting Pressure Velocity | 0.771 MPa-m/sec | 22000 psi-ft/min | 1000 fpm |
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta.. |