Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.04 MPa-m/sec
29700 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data)
Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good ..