Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.00343 - 0.00352 MPa-m/sec | 97.9 - 100 psi-ft/min | 3 m/min |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |