Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 12.0 MPa-m/sec | 343000 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 12.0 MPa-m/sec | 343000 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo VESPEL® SP22 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |